Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0403 W/m-K | 0.280 BTU-in/hr-ft²-°F | ASTM-C-518 |
Saint-Gobain Norton® V740 Multipurpose Pressure Sensitive Adhesive Sealant Foam Description: Medium Density, Multipurpose Foam: Norseal V740 is a closed-cell polyvinyl chloride foam sealant with pressure-sensitive adhesive on one side designed to provide an economical solution .. |
|||
Thermal Conductivity | 0.0403 W/m-K | 0.280 BTU-in/hr-ft²-°F | ASTM-C-518 |
Saint-Gobain Norton® V780 Medium-Density Pressure Sensitive Adhesive Sealant Foam Description: Improved Performance: Norseal® V780 medium density foam sealant combines a closed cell foam substrate with a one-sided pressure-sensitive adhesive. Norseal has been specially formula.. |
|||
Thermal Conductivity | 0.0404 W/m-K | 0.280 BTU-in/hr-ft²-°F | mean temp of 10°C; ISO 8302 1991 |
Zotefoams Evazote® EV50 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |