Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 97.2 µm/m-°C @Temperature -40.0 - 149 °C |
54.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Acetron® POM-C Copolymer Acetal, Porosity-Free, Unfilled, Extruded |
|||
CTE, linear | 97.2 µm/m-°C @Temperature -40.0 - 176 °C |
54.0 µin/in-°F @Temperature -40.0 - 349 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylac® HF143 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
CTE, linear | 97.2 µm/m-°C | 54.0 µin/in-°F | ASTM D696 |
Quantum Acetal-Copolymer Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 97.2 µm/m-°C @Temperature 20.0 °C |
54.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Dielux® PTFE filled Acetal Copolymer Dielux PTFE filled acetal copolymer is an outstanding bearing and wear material for use in both wet and dry environments. It is frequently used in place of traditional metal and plastic bearing mat.. |
|||
CTE, linear | 97.2 µm/m-°C @Temperature 100 °C |
54.0 µin/in-°F @Temperature 212 °F |
ASTM E-831 (TMA) |
Technetics Group Amicon™ Acetal Copolymer
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |