Polymer Property : CTE, linear = 86.7 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 156 µm/m-°C

@Temperature 20.0 °C
86.7 µin/in-°F

@Temperature 68.0 °F
Dow Pellethane® 2103-90AEF Polyurethane Elastomer, Ether Based  (discontinued **)
PELLETHANE® 2103-90AEF elastomer is a polytetramethylene glycol ether based polyurethane elastomer, featuring superior resilience, low temperature properties, excellent hydrolytic stability, and re..
CTE, linear 156 µm/m-°C

@Temperature 20.0 °C
86.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Lubrizol Estane® 2103-90AEFH Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product ..
CTE, linear 156 µm/m-°C
86.7 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® OG142 UV Cure Optical Epoxy
Material Description: A single component, UV curable epoxy, designed for adhesive, sealing, and encapsulating applications found in semiconductor, electro-optics, fiber optics, medical, and scientif..