Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 156 µm/m-°C @Temperature 20.0 °C |
86.7 µin/in-°F @Temperature 68.0 °F |
|
Dow Pellethane® 2103-90AEF Polyurethane Elastomer, Ether Based
(discontinued **) PELLETHANE® 2103-90AEF elastomer is a polytetramethylene glycol ether based polyurethane elastomer, featuring superior resilience, low temperature properties, excellent hydrolytic stability, and re.. |
|||
CTE, linear | 156 µm/m-°C @Temperature 20.0 °C |
86.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Lubrizol Estane® 2103-90AEFH Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film resin for injection blow moldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane product .. |
|||
CTE, linear | 156 µm/m-°C | 86.7 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® OG142 UV Cure Optical Epoxy Material Description: A single component, UV curable epoxy, designed for adhesive, sealing, and encapsulating applications found in semiconductor, electro-optics, fiber optics, medical, and scientif.. |