Polymer Property : CTE, linear = 86.6 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 86.6 µm/m-°C

@Temperature -40.0 - 37.8 °C
48.1 µin/in-°F

@Temperature -40.0 - 100 °F
ASTM E831
Ensinger TECANYL™ MT Autoclavable Polymer
TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease..
CTE, linear 86.6 µm/m-°C

@Temperature -40.0 - 37.8 °C
48.1 µin/in-°F

@Temperature -40.0 - 100 °F
ASTM E831
Ensinger TECANYL™ MT CF30 Autoclavable Polymer
TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease..
CTE, linear 86.6 µm/m-°C

@Temperature -40.0 - 37.8 °C
48.1 µin/in-°F

@Temperature -40.0 - 100 °F
ASTM E831
Ensinger TECANYL™ MT XRO Autoclavable Polymer
TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease..