Thermal Properties Metric English Comments
CTE, linear 84.6 µm/m-°C

@Temperature -40.0 - 149 °C
47.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Acetron® POM-H Homopolymer Acetal, Unfilled, Extruded (ASTM Product Data Sheet)
CTE, linear 84.6 µm/m-°C
47.0 µin/in-°F
ASTM D696
Teknor Apex Chemlon® 253 Nylon 6, Toughened
Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation ..
CTE, linear 84.6 µm/m-°C

@Temperature 20.0 °C
47.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Pomalux® Acetal Copolymer
Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining par..
CTE, linear 84.6 µm/m-°C
47.0 µin/in-°F
TriStar TriSteel PR Metal Backed PTFE Bearing System
Ultraflon 602e enhanced PTFE (PR) lined metal backed bearing , high speed reciprocating, self lubricating, high temperature and high load applications. Liner is designed specifically for high freque..
CTE, linear 84.6 µm/m-°C
47.0 µin/in-°F
TriStar TriSteel PT Metal Backed PTFE Bearing System
Ultraflon 602 (PT) PTFE lined metal backed bearing system, low friction, high PV, high speed sleeve, flange and thrust bearings, zero lube required, high operating temperature. Ultraflon 602 PTFE Li..
CTE, linear 84.6 µm/m-°C

@Temperature 20.0 °C
47.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Ensinger Tecaform™ Acetal Copolymer - Extruded Products (POM)
Tecaform™ is a semi-crystalline thermoplastic offering high strength, stiffness and toughness. It is resistant to hot water, hydrocarbons and solvents, and it posses good bearing and wear properti..
CTE, linear 84.6 µm/m-°C
47.0 µin/in-°F
ASTM D696
Ensinger Tecaform™ FG Blue Food Grade Acetal (POM)
Tecaform™ is resistant to hot water and typical cleaning chemicals. It possesses good bearing and wear properties. The blue color makes it more visible than standard grades. It is commonly used ..
CTE, linear 84.6 µm/m-°C

@Temperature 100 °C
47.0 µin/in-°F

@Temperature 212 °F
ASTM E-831 (TMA)
Technetics Group Amicon™ Acetal Homopolymer  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)