Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake Plastics Pomalux® Acetal Copolymer

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Westlake Plastics
Trade Name Pomalux®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Pomalux® Acetal Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pomalux is a high performance acetal copolymer that has excellent mechanical, electrical, and wear properties. It is engineered to provide outstanding dimensional stability, even when machining parts with complex geometries. It is a good choice for many bearing and wear applications since it has a low coefficient of friction and wears well in both wet and dry environments. Information provided by Westlake Plastics.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Water Absorption 0.22 %
0.22 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D7852
Tensile Strength, Yield 60.7 MPa
8800 psi
ASTM D638
Elongation at Break 75 %
75 %
ASTM D638
Tensile Modulus 2.83 GPa
410 ksi
ASTM D638
Flexural Modulus 2.59 GPa
375 ksi
ASTM D790
Compressive Strength 110 MPa
16000 psi
ASTM D695; at 10% Deflection
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 84.6 µm/m-°C

@Temperature 20.0 °C
47.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.231 W/m-K
1.60 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 157 °C
315 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
219 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0590 in
Electrical Properties Metric English Comments
Dielectric Constant 3.8

@Frequency 60 Hz
3.8

@Frequency 60 Hz
ASTM D150
Users viewing this material also viewed the following: