Thermal Properties Metric English Comments
CTE, linear 152.2 µm/m-°C

@Temperature 20.0 °C
84.56 µin/in-°F

@Temperature 68.0 °F
ASTM E-831
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU)
A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility Elasthane™ TPU exhibits outstanding hydrolytic stabilit..