Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 152.2 µm/m-°C @Temperature 20.0 °C |
84.56 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
DSM Biomedical Elasthane™ 55D Thermoplastic Polyether Polyurethane (TPU) A high tensile strength, aromatic biomedical polymer with an exceptional combination of mechanical properties plus biological compatibility