Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 15.8 µm/m-°C @Temperature 20.0 °C |
8.78 µin/in-°F @Temperature 68.0 °F |
|
California Fine Wire Nickel Alloy 180 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
CTE, linear | 15.8 µm/m-°C @Temperature 20.0 - 95.0 °C |
8.78 µin/in-°F @Temperature 68.0 - 203 °F |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Level 1 Cold Worked Level 1 Cold Worked applies to tensile properties of 0.25 to 4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was origin.. |
|||
CTE, linear | 15.8 µm/m-°C @Temperature 20.0 - 95.0 °C |
8.78 µin/in-°F @Temperature 68.0 - 203 °F |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Level 2 Cold Worked Level 2 Cold Worked applies to tensile and hardness properties of 0.25 to 4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic all.. |
|||
CTE, linear | 15.8 µm/m-°C @Temperature 20.0 - 95.0 °C |
8.78 µin/in-°F @Temperature 68.0 - 203 °F |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Level 3 Cold Worked Level 3 Cold Worked applies to tensile properties of 0.25 to 2.4 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was orig.. |
|||
CTE, linear | 15.8 µm/m-°C @Temperature 20.0 - 95.0 °C |
8.78 µin/in-°F @Temperature 68.0 - 203 °F |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Annealed Annealed applies to tensile and/or hardness; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was originally designed as a high tempe.. |
|||
CTE, linear | 15.8 µm/m-°C @Temperature 20.0 - 95.0 °C |
8.78 µin/in-°F @Temperature 68.0 - 203 °F |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Level 4 Cold Worked Level 4 Cold Worked applies to tensile properties of 0.25 to 2 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was origin.. |
|||
CTE, linear | 15.8 µm/m-°C @Temperature 20.0 - 95.0 °C |
8.78 µin/in-°F @Temperature 68.0 - 203 °F |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Level 5 Cold Worked Level 5 Cold Worked applies to tensile properties of 0.25 to 1.5 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was orig.. |