Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 15.72 µm/m-°C @Temperature 20.0 - 500 °C |
8.733 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum AL 304DA Stainless/Carbon Steel Three-Ply Composite Composition above represents only the Type 304 cladding. Its iron content calculated as balance.Allegheny Ludlum AL 304DA is tri-ply composite consisting of a dual stabilized, low carbon steel cent.. |