Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 782 µm/m-°C @Temperature 20.0 °C |
435 µin/in-°F @Temperature 68.0 °F |
|
Paratherm Corporation Paratherm™ MR Heat Transfer Fluid Description: Paratherm MR® is a mid-range heat transfer fluid. It is efficient across the temperature range, thermally stable and cost-effective. Non-aromatic and non-toxic, the fluid is safe to .. |