Polymer Property : CTE, linear = 435 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 782 µm/m-°C

@Temperature 20.0 °C
435 µin/in-°F

@Temperature 68.0 °F
Paratherm Corporation Paratherm™ MR Heat Transfer Fluid
Description: Paratherm MR® is a mid-range heat transfer fluid. It is efficient across the temperature range, thermally stable and cost-effective. Non-aromatic and non-toxic, the fluid is safe to ..