Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
78.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Owens Corning Glass Fiber Reinforced Polyurethane, Milled Fibers (RRIM), 13 wt.% glass Polyurethane is normally used for its structural properties when molded. It is highly resistant to most organic solvents. It is not recommended for use with strong acids and alkalis, steam, fuels, a.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
78.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (DAM) Information provided by Ravago |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
78.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ravago Manufacturing Americas Hylon® N1000STL Nylon 6/6 (DAM)
(discontinued **) Information provided by Entec. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
78.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Kynar® 2850 PVDF Copolymer Manufactured from Kynar® polyvinylidene fluoride resin. This material offers excellent corrosion and chemical resistance at both ambient and elevated temperatures, PVDF is also inherently UV stab.. |