Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 137 µm/m-°C @Temperature 20.0 °C |
76.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Bayflex® 190 Polyurethane Elastomeric RIM, 20% Mica Filled, MDI-based 2-Component Liquid System 0.150 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |