Thermal Properties Metric English Comments
CTE, linear 137 µm/m-°C

@Temperature 20.0 °C
76.1 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Covestro Bayflex® 190 Polyurethane Elastomeric RIM, 20% Mica Filled, MDI-based 2-Component Liquid System
0.150 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o..