Thermal Properties Metric English Comments
CTE, linear 48.0 - 74.4 µm/m-°C
26.7 - 41.3 µin/in-°F
Average value: 65.6 µm/m-°C Grade Count:26
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..