Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.9 µm/m-°C @Temperature 20.0 - 100 °C |
7.72 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals MONEL® Alloy 400 A nickel-copper alloy with high strength and excellent corrosion resistance in a range of media including sea water, hydrofluoric acid, sulfuric acid, and alkalis. Used for marine engineering, chem.. |
|||
CTE, linear | 13.9 µm/m-°C @Temperature 25.0 - 500 °C |
7.72 µin/in-°F @Temperature 77.0 - 932 °F |
|
Wieland Porta SMK 82 PFM Alloy Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, removable partials, ceramic veneering, acrylic veneeringDental |
|||
CTE, linear | 13.9 µm/m-°C @Temperature 20.0 °C |
7.72 µin/in-°F @Temperature 68.0 °F |
alloy 600 property |
Arlon I51576R015 Silicone Rubber/Fiberglass/Alloy Laminate Top layer of side 2: alloy 600 foil; Bottom layer of side 2: cured silicone rubber; Substrate is 7628 fiberglass; Side 1: cured silicone rubber |