Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 124 - 124 µm/m-°C @Temperature 60.0 - 138 °C |
68.9 - 68.9 µin/in-°F @Temperature 140 - 280 °F |
Average value: 124 µm/m-°C Grade Count:1 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |