Polymer Property : CTE, linear = 6.65 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 6.65 µm/m-°C

@Temperature 260 °C
3.69 µin/in-°F

@Temperature 500 °F
Fired Thermal Expansion
Ferro EG 2004 Low-Temperature Sealing
VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp..
CTE, linear 6.65 µm/m-°C

@Temperature 260 °C
3.69 µin/in-°F

@Temperature 500 °F
Ferro EG 2928 Glaze and Sealant Glass
Glass Type: Pb-Zn-B Typical Powder Form: VEG, MVG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective an..