Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.65 µm/m-°C @Temperature 260 °C |
3.69 µin/in-°F @Temperature 500 °F |
Fired Thermal Expansion |
Ferro EG 2004 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |
|||
CTE, linear | 6.65 µm/m-°C @Temperature 260 °C |
3.69 µin/in-°F @Temperature 500 °F |
|
Ferro EG 2928 Glaze and Sealant Glass Glass Type: Pb-Zn-B Typical Powder Form: VEG, MVG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective an.. |