Polymer Property : CTE, linear = 6.35 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 6.35 µm/m-°C

@Temperature 260 °C
3.53 µin/in-°F

@Temperature 500 °F
Ferro EG 2964 Glaze and Sealant Glass
Glass Type: Bi-Zn-B Typical Powder Form: VWG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and ins..