Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.35 µm/m-°C @Temperature 260 °C |
3.53 µin/in-°F @Temperature 500 °F |
|
Ferro EG 2964 Glaze and Sealant Glass Glass Type: Bi-Zn-B Typical Powder Form: VWG Typical Application: ZnO, Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and ins.. |