Polymer Property : CTE, linear = 57.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 30.0 - 57.0 µm/m-°C

@Temperature 50.0 - 300 °C
16.7 - 31.7 µin/in-°F

@Temperature 122 - 572 °F
Average value: 42.7 µm/m-°C Grade Count:9
Overview of materials for Polyimide, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app..