Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 5.80 µm/m-°C @Temperature 260 °C |
3.22 µin/in-°F @Temperature 500 °F |
Fired Thermal Expansion |
Ferro CF 7578 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: VSD Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific .. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 25.0 - 600 °C |
3.22 µin/in-°F @Temperature 77.0 - 1110 °F |
|
ICE Hot Pressed SiC Data provided by the manufacturer, International Ceramic Engineering. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 20.0 - 1000 °C |
3.22 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Goodfellow Ruby, Al2O3 Ruby exhibits identical properties to those of sapphire. Small amounts of impurities, especially chromium oxide, give ruby a red coloration. Useful optical range from 150 - 5500 nm.Information pro.. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 1000 °C |
3.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SF35 Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 1000 °C |
3.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SF36 Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 1000 °C |
3.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CH-2 Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 1000 °C |
3.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CH-3 Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 1000 °C |
3.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CH-S Hard Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 1000 °C |
3.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories N5 Fireclay brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 5.80 µm/m-°C @Temperature 20.0 - 1000 °C |
3.22 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Anderman Ceramics EM80P Corundum Porous synthetic mullite with very high thermal shock. Available as tube, sheath, or rod up to 10 ft (3 m) long with diameters 0.3" to 20".Information provided by Anderman Ceramics. |
|||
CTE, linear | 5.80 µm/m-°C @Temperature -30.0 - 300 °C |
3.22 µin/in-°F @Temperature -22.0 - 572 °F |
average, isotropic |
AGY ADVANTEX® Generic Glass Fiber OC/AGY E-CR glass. Various silanes and starch oil are used as binders. Acid resistant. Lower alkali resistance than VeTron® and ZenTron® glass fibers.Information provided by AGY Holding Corp... |