Thermal Properties Metric English Comments
CTE, linear 9.20 µm/m-°C

@Temperature 20.0 °C
5.11 µin/in-°F

@Temperature 68.0 °F
Hogen Duralloy H30W 80 Tungsten/20 Copper PM Metal Composite
RWMA Class 12.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 12 material is ..
CTE, linear 9.20 µm/m-°C

@Temperature 20.0 °C
5.11 µin/in-°F

@Temperature 68.0 °F
MarkeTech Lanthanum Aluminum Oxide (LaAlO3) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
CTE, linear 9.19 µm/m-°C
5.11 µin/in-°F
c direction
MarkeTech Rutile (TiO2) Fiber Optic Crystal
More chemically and physically resistant than Yttrium Vanadate. Large birefringence. Used for fiber optic beam displacers and optical isolators. Grown by Vernull method. Transmission range 500 to..
CTE, linear 9.20 µm/m-°C

@Temperature 20.0 °C
5.11 µin/in-°F

@Temperature 68.0 °F
MarkeTech Thorium-Doped Lanthanum Aluminum Oxide (Th:LaAlO3) Single Crystal Substrate
Data provided by MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
CTE, linear 9.20 µm/m-°C

@Temperature 260 °C
5.11 µin/in-°F

@Temperature 500 °F
Ferro F 1040 Metal Sealing
Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Compress.Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched se..
CTE, linear 9.20 µm/m-°C

@Temperature 20.0 - 300 °C
5.11 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott Glass 8625 Biocompatible Glass
Biocompatible glass, high IR-absorbing, Transponders (implantable) The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by S..
CTE, linear 9.20 µm/m-°C

@Temperature 260 °C
5.11 µin/in-°F

@Temperature 500 °F
Fired Thermal Expansion
Ferro CF 7572 Low-Temperature Sealing
DEVITRIFYING Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet speci..