MarkeTech Lanthanum Aluminum Oxide (LaAlO3) Single Crystal Substrate

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer MarkeTech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech Lanthanum Aluminum Oxide (LaAlO3) Single Crystal Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
Physical Properties Metric English Comments
Density 6.51 g/cc
0.235 lb/in³
a Lattice Constant 3.79 Ã…
3.79 Ã…
c Lattice Constant 13.11 Ã…
13.11 Ã…
Thermal Properties Metric English Comments
CTE, linear 9.20 µm/m-°C

@Temperature 20.0 °C
5.11 µin/in-°F

@Temperature 68.0 °F
Melting Point 2180 °C
3960 °F
Electrical Properties Metric English Comments
Dielectric Constant 24.5
24.5