Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 85.5 µm/m-°C | 47.5 µin/in-°F | |
Hexcel® HexPly® F185 Epoxy Resin HexPly® F185 is an advanced epoxy formulation designed for autoclave curing to offer very high sandwich and metal bonding strengths with moderate laminate strengths. HexPly® F185 is a structural a.. |