Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hexcel® HexPly® F185 Epoxy Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® F185 Epoxy Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® F185 is an advanced epoxy formulation designed for autoclave curing to offer very high sandwich and metal bonding strengths with moderate laminate strengths. HexPly® F185 is a structural adhesive and co-curing grade epoxy resin with a 250ºF (121ºC) cure This system offers the highest available fracture toughness and strain to failure of the 250ºF (121ºC) cure resins.Information provided by HexCel
Physical Properties Metric English Comments
Specific Gravity 1.286 g/cc
1.286 g/cc
Moisture Absorption at Equilibrium 7.0 %
7.0 %
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
Elongation at Yield >= 9.5 %
>= 9.5 %
Tensile Modulus 2.90 GPa
421 ksi
Fracture Toughness 3.69 MPa-m½
3.36 ksi-in½
Thermal Properties Metric English Comments
CTE, linear 85.5 µm/m-°C
47.5 µin/in-°F
Glass Transition Temp, Tg 77.0 °C
171 °F
Dry
Processing Properties Metric English Comments
Gel Time 5.00 - 11.0 min

@Temperature 121 °C
5.00 - 11.0 min

@Temperature 250 °F