Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 66.0 - 84.6 µm/m-°C | 36.7 - 47.0 µin/in-°F | Average value: 81.3 µm/m-°C Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo.. |