Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 41.2 µm/m-°C | 22.9 µin/in-°F | |
BCC Products MB 5000 Urethane Tooling Board MB 5000 is an extremely tough, high impact Urethane Plank, that can be used for metal forming as well as nickel plating mandrels. Features: excellent machinability, low dust emission, mostly shavin.. |