Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 22.9 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 41.2 µm/m-°C
22.9 µin/in-°F
BCC Products MB 5000 Urethane Tooling Board
MB 5000 is an extremely tough, high impact Urethane Plank, that can be used for metal forming as well as nickel plating mandrels. Features: excellent machinability, low dust emission, mostly shavin..
Copyright © lookpolymers.com All Rights Reserved