Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 69.5 µm/m-°C @Temperature 20.0 °C |
38.6 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
CPC - Vycom Corzan® CPVC Chlorinated PVC Corzan CPVC is a high heat, corrosion resistant chlorinated polyvinyl chloride (CPVC) sheet. Because of its excellent corrosion resistance at elevated temperatures, it is ideally suited for self-sup.. |
|||
CTE, linear | 69.5 µm/m-°C | 38.6 µin/in-°F | T<Tg; ASTM E831-93 |
3D Systems Accura® accuGen™ HC and Ar Plastic for the SLA® 250 System Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® 250 system.Typical ApplicationsMulti-purpose modelsRTV mold patternsForm/Fit/.. |