Thermal Properties Metric English Comments
CTE, linear 17.0 - 68.4 µm/m-°C
9.44 - 38.0 µin/in-°F
Average value: 34.6 µm/m-°C Grade Count:15
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
CTE, linear 37.8 - 68.4 µm/m-°C
21.0 - 38.0 µin/in-°F
Average value: 55.0 µm/m-°C Grade Count:13
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..