Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 34.9 µm/m-°C | 19.4 µin/in-°F | |
Atom Adhesives AA-DUCT 2919 Epoxy Adhesive AA-DUCT 2919 is a non-bleeding, electrically conductive, silver-filled epoxy formulation recommended for electronic bonding, coating, and sealing applications that require good flexibility coupled w.. |