Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 61.2 µm/m-°C @Temperature 20.0 °C |
34.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Lubri-Tech™ PF-000/15T Polysulfone, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
CTE, linear | 61.2 µm/m-°C @Temperature 20.0 °C |
34.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
ITW Devcon Metal Repair Stainless Steel Putty (ST), Grey Information provided by ITW Devcon |
|||
CTE, linear | 61.2 µm/m-°C @Temperature 20.0 °C |
34.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
ITW Devcon Plastic Steel® Metal Repair 5 Minute® Putty (SF), Dark Grey Information provided by ITW Devcon |
|||
CTE, linear | 61.2 µm/m-°C | 34.0 µin/in-°F | ASTM D696 |
Teknor Apex Chemlon® 223 Nylon 6, Unreinforced Features: Nucleated for fast cyclingProcessing Method: Injection MoldingForms: Pellets Additive: Nucleating AgentInformation Provided by Teknor Apex |
|||
CTE, linear | 61.2 µm/m-°C | 34.0 µin/in-°F | ASTM D696 |
Teknor Apex Chemlon® 212 Nylon 6, Unreinforced Features: Lubricated, General Purpose; General purpose nylon 6; Slightly tougher and more ductile than nylon 66 Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex.. |
|||
CTE, linear | 61.2 µm/m-°C @Temperature 20.0 °C |
34.0 µin/in-°F @Temperature 68.0 °F |
ASTM D1525 |
PlastxWorld CEVIAN® S1210 PC/ABS alloy Glass fiber reinforced PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
CTE, linear | 61.2 µm/m-°C | 34.0 µin/in-°F | ASTM D696 |
Ensinger Hydex™ 301 Rigid Polyurethane (PU) Hydex™ 301 is clear totally rigid polyurethane. It combines excellent clarity when polished with a broad range of chemical resistance and outstanding practical toughness. |
|||
CTE, linear | 61.2 - 108 µm/m-°C | 34.0 - 60.0 µin/in-°F | Average value: 84.7 µm/m-°C Grade Count:13 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |