Material Notes:
Hydex™ 301 is clear totally rigid polyurethane. It combines excellent clarity when polished with a broad range of chemical resistance and outstanding practical toughness.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.19 %

@Time 86400 sec
0.19 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 62.1 MPa
9000 psi
ASTM D638
Tensile Strength, Yield 68.9 MPa
10000 psi
ASTM D638
Elongation at Break 140 %
140 %
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Tensile Modulus 2.14 GPa
310 ksi
ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm
2.40 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.21
0.21
SS counter surface
Coefficient of Friction, Static 0.22
0.22
SS counter surface
Thermal Properties Metric English Comments
CTE, linear 61.2 µm/m-°C
34.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
220 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C
170 °F
ASTM D648
Vicat Softening Point 109 °C
228 °F
ASTM D1525