Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 35.0 - 59.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
19.4 - 32.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |