Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 19.8 - 30.1 µm/m-°C @Temperature 20.0 °C |
11.0 - 16.7 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Network Polymers Kepital® F20-25 Description: Natural Acetal Copolymer, 25% Glass Reinforced GradeInformation provided by Network Polymers Inc. |