Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 26.7 µm/m-°C | 14.8 µin/in-°F | |
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining.. |
|||
CTE, linear | 26.7 µm/m-°C | 14.8 µin/in-°F | |
Magnesium Elektron Elektron® 43 Magnesium Wrought Alloy High strength wrought Mg alloy available as rolled plate, forging feedstock, and extrusions. It is a wrought evolution of the casting alloy Elektron WE43. Elektron 43 uses zirconium grain refining.. |