Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 236 µm/m-°C | 131 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 310M-T Flexible Epoxy Material Description: A two component, flexible epoxy designed for low stress applications in semiconductor, hybrid, medical, acoustical and optical industries. Replacement for EPO-TEK® 310T.Info.. |