CTE, linear 22.5 µm/m-°C

@Temperature 20.0 - 1000 °C
12.5 µin/in-°F

@Temperature 68.0 - 1830 °F
Goodfellow Dural® Aluminum /Copper/Magnesium Alloy
High strength, low weight alloy; in the solution heat-treated and aged condition, mechanical properties are as good as, or better than, low-carbon steel. Limited weldability. Used in aircraft and ae..
CTE, linear 22.5 µm/m-°C

@Temperature 20.0 - 100 °C
12.5 µin/in-°F

@Temperature 68.0 - 212 °F
Aleris Weldural Aluminum Alloy, 400 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
CTE, linear 22.5 µm/m-°C

@Temperature 20.0 - 100 °C
12.5 µin/in-°F

@Temperature 68.0 - 212 °F
Aleris Weldural Aluminum Alloy, 600 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
CTE, linear 22.5 µm/m-°C

@Temperature 20.0 - 100 °C
12.5 µin/in-°F

@Temperature 68.0 - 212 °F
Aleris Weldural Aluminum Alloy, 100 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
CTE, linear 22.5 µm/m-°C

@Temperature 20.0 - 100 °C
12.5 µin/in-°F

@Temperature 68.0 - 212 °F
Aleris Weldural Aluminum Alloy, 200 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
CTE, linear 22.5 µm/m-°C

@Temperature 20.0 - 100 °C
12.5 µin/in-°F

@Temperature 68.0 - 212 °F
Aleris Weldural Aluminum Alloy, 300 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
CTE, linear 22.5 µm/m-°C

@Temperature 20.0 - 100 °C
12.5 µin/in-°F

@Temperature 68.0 - 212 °F
Aleris Weldural Aluminum Alloy, 500 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..
CTE, linear 22.5 µm/m-°C

@Temperature 20.0 - 100 °C
12.5 µin/in-°F

@Temperature 68.0 - 212 °F
Aleris Weldural Aluminum Alloy, 700 mm Thickness
Sample treatment not specified for property data.Applications include precise mechanical parts with high dimensional stability, machine components, molds, and refrigeration engineering. Good weldab..