Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 21.8 µm/m-°C @Temperature 20.0 °C |
12.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Zelux® 30% GF Polycarbonate 30% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |