Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 21.8 µm/m-°C

@Temperature 20.0 °C
12.1 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Westlake Plastics Zelux® 30% GF Polycarbonate 30% Glass Filled
Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and ..