Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 21.2 µm/m-°C | 11.8 µin/in-°F | |
BCC Products BC 5008-2 General Purpose Epoxy System BC 5008-2 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC 5008-2 is a clear, amber, medium pot life material, with heat resistance to 175ºF. A.. |