Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 2.33 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear >= 4.20 µm/m-°C

@Temperature 20.0 °C
>= 2.33 µin/in-°F

@Temperature 68.0 °F
MarkeTech AN 180 Aluminum Nitride Ceramic Substrate, 99% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ..
CTE, linear 4.20 µm/m-°C

@Temperature 25.0 - 1000 °C
2.33 µin/in-°F

@Temperature 77.0 - 1830 °F
ASTM C372
CoorsTek AIN-170 Hot Pressed Aluminum Nitride
Aluminum Nitride Advantages: High heat dissipation with thermal conductivity of 170 W/m K Non-toxic alternative to BeO Thermal expansion coefficient similar to Si, GaN, and GaAs semiconductors H..
CTE, linear 4.20 µm/m-°C

@Temperature 1000 °C
2.33 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SBN-1 Bricks, Reaction Bonded SiC
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 4.20 µm/m-°C

@Temperature 1000 °C
2.33 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SF31S Hard Fireclay brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 4.20 µm/m-°C
2.33 µin/in-°F
Volumetric thermal expansion
China-Yixing Longly Refractories ASM-120 Cordierite-Mullite
Featured mullite, cordierite as the main raw material, the use of advanced production technology, professionally manufacturing the kiln furniture of ceramic and powder metallurgy with load bearing b..
CTE, linear 4.20 - 4.80 µm/m-°C

@Temperature 25.0 - 800 °C
2.33 - 2.67 µin/in-°F

@Temperature 77.0 - 1470 °F
China-Yixing Longly Refractories ZTA (10%ZrO2) Zirconia Toughened Alumina Composite Ceramic
LONGLY's Zirconia Toughened Alumina ceramics (hereafter referred as composite ceramic, ZTA) is white, corrosion resistance, good chemical stability. As well all know that alumina is hard, while zir..
CTE, linear 4.20 µm/m-°C

@Temperature 20.0 - 200 °C
2.33 µin/in-°F

@Temperature 68.0 - 392 °F
CeramTec Rubalit® A 1896 brown Alumina
CeramTec AG's seal and regulator discs are made mainly of Rubalit® A 1896, a material developed especially for this application that is noted for the following special properties: outstanding hard..
Copyright © lookpolymers.com All Rights Reserved