Polymer Property : CTE, linear = 194 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 350 - 400 µm/m-°C
194 - 222 µin/in-°F
Master Bond MasterSil 153Med Silicone Paste for Medical Applications
Description: Master Bond MasterSil 153Med is a two component silicone compound with a paste consistency for high performance bonding and sealing. It can be used for medical device applications as it..