Master Bond MasterSil 153Med Silicone Paste for Medical Applications

Category Polymer , Thermoset , Silicone
Manufacturer Master Bond Inc.
Trade Name Mastersil
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond MasterSil 153Med Silicone Paste for Medical Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Master Bond MasterSil 153Med is a two component silicone compound with a paste consistency for high performance bonding and sealing. It can be used for medical device applications as it meets USP Class VI testing and ISO 10993-5 for cytotoxicity. MasterSil 153Med is an addition cured system and does not require exposure to air for cross-linking. It has a convenient one to one mix ratio by weight, and will not outgas while curing. It is 100% solids and contains no solvents. MasterSil 153Med exhibits typical silicone flexibility and high temperature resistance. MasterSil 153Med has a long working life and very low exotherm. It bonds well to a wide variety of substrates including most metals, many plastics, glass and ceramic. Most importantly, it will bond well to cured silicone rubber. It has good electrical insulation properties. Its flexibility allows it to withstand severe thermal cycling and resist vibration and shock. It has a self priming feature that enhances the bonding properties of the system. Also, it is very water resistant. MasterSil 153Med is translucent and is serviceable over the broad temperature range of -65°F to +400°F. It is widely used in medical device applications where high flexibility and splendid temperature resistance are required. Product Advantages: Addition cured; no by-products released during cure; does not require air for curing. Low exotherm; very long pot life. Very low shrinkage upon cure. Readily cures at ambient temperatures or faster cure at elevated temperatures. Softer durometer; offers repairability. Bonds well to a variety of substrates including silicone rubber. Self priming feature. Good electrical insulation properties; highly resistant to water. Outstanding flexibility combined with high temperature resistance. Meets USP Class VI and ISO 10993-5 specifications. Key Features Passes USP Class VI testing Addition cured system Self priming feature Meets ISO 10993-5 specifications Serviceable from -65°F to +400°F Paste consistencyInformation provided by MasterBond®
Physical Properties Metric English Comments
Viscosity >= 200000 cP
>= 200000 cP
Part B
>= 350000 cP
>= 350000 cP
Part A
Mechanical Properties Metric English Comments
Hardness, Shore A 20 - 35
20 - 35
Tensile Strength at Break 2.76 - 3.45 MPa
400 - 500 psi
Elongation at Break 400 - 500 %
400 - 500 %
Shear Strength >= 1.38 MPa
>= 200 psi
Tensile lap, Al to Al
Thermal Properties Metric English Comments
CTE, linear 350 - 400 µm/m-°C
194 - 222 µin/in-°F
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Constant 2.9

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
2.9

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Dielectric Strength 17.7 kV/mm

@Thickness 3.17 mm
450 kV/in

@Thickness 0.125 in
Processing Properties Metric English Comments
Cure Time 120 - 180 min

@Temperature 93.3 °C
2.00 - 3.00 hour

@Temperature 200 °F
2880 - 4320 min

@Temperature 23.9 °C
48.0 - 72.0 hour

@Temperature 75.0 °F
Pot Life 5.0 - 7.0 min
5.0 - 7.0 min
100 gram batch
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
in original unopened containers
Descriptive Properties Value Comments
Mixing Ratio (A to B) 1:1
by weight