Thermal Properties Metric English Comments
CTE, linear 16.5 - 19.2 µm/m-°C

@Temperature -60.0 - 60.0 °C
9.17 - 10.7 µin/in-°F

@Temperature -76.0 - 140 °F
Mateck Barium Fluoride, BaF2
Optical crystals