Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 16.5 - 19.2 µm/m-°C @Temperature -60.0 - 60.0 °C |
9.17 - 10.7 µin/in-°F @Temperature -76.0 - 140 °F |
|
Mateck Barium Fluoride, BaF2 Optical crystals |
|||
CTE, linear | 16.5 - 19.4 µm/m-°C @Temperature -60.0 - 60.0 °C |
9.17 - 10.8 µin/in-°F @Temperature -76.0 - 140 °F |
|
Mateck Calcium Fluoride (CaF2) Optical crystals |
|||
CTE, linear | 16.5 - 17.7 µm/m-°C @Temperature 20.0 - 700 °C |
9.17 - 9.83 µin/in-°F @Temperature 68.0 - 1290 °F |
|
Advanced Ceramics MEXIM C ACL 2091 Mexim C has been specially formulated to give an expansion closely matched to that of copper. It has high electrical insulation properties and good mechanical strength, and finds increasing applicat.. |